Table 5.

Interpore distances for AAO tubular membranes anodized by 2.7% oxalic acid at 30 and 40 V at 0°C

Concentration of oxalic acid (wt %) Interpore Distance (nm)
Voltage (V)
30 40
2.7 65.1±6.5. 80.5±3.2