Skip to main content
. 1998 Apr;9(4):715–731. doi: 10.1091/mbc.9.4.715

Figure 9.

Figure 9

Rubber substrate contractility assay. GD25, GD25-β1B, and GD25-β1A cells were plated for 1 d on silicone rubber substrata and photographed under phase contrast. Note the incapacity of GD25-β1B cells to wrinkle the silicon substrate. Bar, 50 μm.