Skip to main content
. Author manuscript; available in PMC: 2008 Dec 1.
Published in final edited form as: Nano Lett. 2007 Nov 13;7(12):3895–3900. doi: 10.1021/nl0724788

Figure 3.

Figure 3

Difference between the conductance after and before streptavidin binding, divided by the conductance before binding of 10 µM streptavidin using 1 h incubation. The signal change is independent on the numbers of nanochannels. For the control measurement the channels were coated with PLL-g-PEG (no biotin), whereas all other chips were pretreated with PLL-g-PEGbiotin.