Skip to main content
. Author manuscript; available in PMC: 2008 Oct 8.
Published in final edited form as: Electroanalysis. 2008 Jan;20(2):115–122. doi: 10.1002/elan.200704040

Fig. 1.

Fig. 1

Tapping mode AFM image of a) PLL film and b) PLL-SWCNT2 film on mica. PLL-SWCNT2 assembly showed average protrusion height of 23 ± 5 nm and average domain width of 382 ± 68 nm. X-axis = 0.2 μm/division; Z-axis = 35 nm/division.