UV-visible spectra for (A) the titration of CdCl2 into a solution of TRIL12DLL16C at pH 8.5 with the characteristic LMCT at λmax 235 nm and (B) the titration curve of absorbance at λmax vs. equivalents of Cd(II) added per trimer for both 10 μM (TRIL12DLL16C)3 and (GRANDL12DLL16CL26AL30C)3max 230 nm) at pH 8.5.