Skip to main content
. Author manuscript; available in PMC: 2008 Dec 9.
Published in final edited form as: Nanotechnology. 2006 Aug 14;17(15):3880–3891. doi: 10.1088/0957-4484/17/15/045

Figure 2.

Figure 2

SEM micrographs of (a) plain PCLEEP fibres, PCLEEP64 6% electrospun at humidity of 68–72%; (b) plain PCL fibres, PCL64 10%; (c) retinoic acid-encapsulated (20 wt%) PCLEEP fibres; and (d) BSA-encapsulated (10 wt%) PCLEEP fibres; and wide-field fluorescent micrographs of (e) retinoic acid-encapsulated (10 wt%) PCLEEP fibres; and (f) FITC-BSA-encapsulated (20 wt%) PCLEEP fibres.