Published in final edited form as: Nanotechnology. 2006 Aug 14;17(15):3880–3891. doi: 10.1088/0957-4484/17/15/045

Figure 6.

Figure 6

(a) Effects of electrospinning process and concentration of polymer solutions used during electrospinning on structure of PCL. XRD pattern of PCL film and electrospun nanofibrous mesh, focusing on 2θ from 16° to 25°. Inset: XRD pattern of PCL film and fibres over a wider 2θ range; and (b) XRD pattern of nanofibres composed of 10 wt% PCL with retinoic acid encapsulation. Inset: XRD pattern of PCLEEP samples, H2O140 (blue) and RA20 (red).