Skip to main content
. Author manuscript; available in PMC: 2010 Jan 1.
Published in final edited form as: Biomaterials. 2008 Oct 26;30(3):409–422. doi: 10.1016/j.biomaterials.2008.09.040

Figure 7.

Figure 7

(A) Representative creep response of glutaraldehyde crosslinked LysB10 films subjected to tensile stress at 45kPa and 450kPa. (B) Creep behavior of glutaraldehyde crosslinked and non-crosslinked LysB10 films at a stress of 45 kPa.