Table 2.

Stress factor range at fatigue crack inception for conventional UHMWPE and vitamin E-doped, irradiated UHMWPE

Sample ΔKincep (MPa m1/2)
Conventional UHMWPE [14] 1.19 ± 0.02
Vitamin E-doped, irradiated UHMWPE [14] 0.77 ± 0.02
100-kGy irradiated and melted UHMWPE [13] 0.56 ± 0.02
Aged conventional UHMWPE [13] 0.18 ± 0.06