Fig. 8.

Fig. 8

Superior endplate of specimen B1 (magnification 10:1) after 10 million cycles (ISOinitial) with oval shaped wear traces on the metallic bearing surface and specimen B2 after 15 million cycles (ASTM) with mainly linear wear traces on the superior metallic bearing surface (magnification 16:1)