Figure 3

Dynamic mechanical analysis of SELPs 47K 4 wt% (◆), 8 wt% (■), and 12 wt% (▲) as well as SELP-415K 12 wt% (×) cured for 4 hours. SELP-47K 12 wt% formed stiff gels that had significantly higher modulus than all other tested gels. SELP-415K 12 wt%, despite forming hydrogels that held their shape unaided, gave results similar to that of the weakest SELP-47K 4 wt% hydrogels.