Figure 4. Profiles of five PDMS membranes spun for 5 min on glass.

Figure 4

Each profile is a single sample, ending in the edge bead. The profiles in Figure 4 were measured from the center point of the slide to the edge along the long axis as indicated by the “Profile line” in Figure 5.