Skip to main content
. Author manuscript; available in PMC: 2009 Mar 9.
Published in final edited form as: Biomaterials. 2007 May 26;28(26):3786–3796. doi: 10.1016/j.biomaterials.2007.05.015

Table 4.

Group 4: effect of strong layer/macroporous layer thickness ratio

Strong layer, a (mm) 0 0.5 1.0 1.5 2.0 2.5 3.0
Macroporous layer, b (mm) 3.0 2.5 2.0 1.5 1.0 0.5 0
a/h ratioa 0 0.17 0.33 0.50 0.67 0.83 1
a

h = a+b, as shown at top of Fig. 7. Other parameters for Table 4 are stated in the text.