Figure 2.

Figure 2

Adhesives formulated with water (A08 and A16) exhibited significantly increased levels of net MAA in PLE (top) and HEMA in PB (bottom) relative to the adhesives formulated without water (A00). Furthermore, the daily release of net MAA in PLE exceeds that of HEMA release in PB for all adhesives.