Figure 2.

Figure 2

Plots of the hardness (a) and fracture toughness (b) of rat incisor enamel in 4 experimental groups, namely, wet untreated, dry untreated, dry treated, and wet treated, collected in the mid-sagittal (■) and transverse (◆) planes. Error bars represent standard deviation values based on data obtained from 3 incisors per compositional group.