Skip to main content
. 2009 Jan 16;10(1):88–97. doi: 10.1208/s12249-008-9179-9

Table II.

Swelling Properties of the Free Polymers

Ratio of ERL/EC (%, w/w) Change in thickness (%) Percentage swelling, I s (%)
100:0 37.7 ± 6.35 129 ± 14.0
50:50 26.6 ± 1.56 73.7 ± 21.8
0:100 7.03 ± 3.46 6.12 ± 5.47

All values are expressed as means ± SD (n = 3)

EC ethyl cellulose, ERL Eudragit RL 100, AZT zidovudine, DBS dibuthyl sebacate