Table 1.

The r1 and r2 relaxivities and relaxivity ratio (r2/r1) of Fe3O4 MNNA and commercial contrast agents: Resovist (SH U 555 A), Feridex (AMI-25) and Supravist (SH U 555 C) measured at 3T [20].

Materials Surface functionality r1
(mM-1s-1)
r2
(mM-1s-1)
r2/r1
Fe3O4 MNNA Amine functionalized Fe3O4 superparamagnetic nanoassemblies 2.2 314.6 143
Resovist (SH U 555 A) Carboxydextran-coated superparamagnetic iron oxide 4.6 143 31.0
Feridex (AMI-25) Dextran-coated superparamagnetic iron oxide 4.1 93 22.6
Supravist (SH U 555 C) Carboxydextran-coated superparamagnetic iron oxide 7.3 57 7.8