Table 1.

Polymer Composition and Concentration and Elastase Effects on Swelling

SELP Analog SELP Concentration Release Media
47K 4% PBS
47K 8% PBS
47K 12% PBS
415K 12% PBS
47K 4% PBS with 100ng Elastase
47K 8% PBS with 100ng Elastase
47K 12% PBS with 100ng Elastase
415K 12% PBS with 100ng Elastase
47K 4% PBS with 10ng Elastase
47K 4% PBS with 50ng Elastase
47K 4% PBS with 150ng Elastase
47K 4% PBS with 200ng Elastase