Skip to main content
. Author manuscript; available in PMC: 2010 Jul 1.
Published in final edited form as: Biomaterials. 2009 Mar 28;30(20):3486–3494. doi: 10.1016/j.biomaterials.2009.03.008

Figure 1.

Figure 1

In vitro release profile of BSA-FITC from polyurethane scaffolds. BSA-FITC was incorporated in the scaffold as solution in the presence of 0.5% glucose, and as powder in presence of different weight percentages of glucose. Each data point represents the mean of three measurements ± SD.