Table 4.

Stress factor range at fatigue crack inception for conventional UHMWPE and a-tocopherol-doped, irradiated UHMWPE

Sample ΔKincep (MPa m1/2)
Conventional UHMWPE 1.19 ± 0.02
a-Tocopherol-doped, irradiated UHMWPE 0.77 ± 0.02
100-kGy irradiated and melted UHMWPE [13] 0.56 ± 0.02