In vitro factor release. DAPT release was analyzed from alginate hydrogels containing 86ng DAPT alone (diamond), 860ng DAPT alone (square), 8600ng DAPT alone (triangle), or 860ng DAPT and 3μg VEGF (horizontal line). VEGF release was monitored from gels containing 3μg VEGF alone (star). Mean values are presented with standard deviations (n=6).