Skip to main content
. Author manuscript; available in PMC: 2010 Mar 1.
Published in final edited form as: Biomaterials. 2008 Dec 25;30(8):1542–1550. doi: 10.1016/j.biomaterials.2008.11.011

Figure 3. Shelf life tests.

Figure 3

Burst pressure tests were performed at different time points after the standard maturation time on TEBVs from four different patients. Vessel strength declined linearly by about 1–2% in burst pressure per week.