A graph shows the dynamic rheology as a function of the frequency for SFs modified by cross-linked HA (Synvisc®) during a 44-day period. Temperature = 25°C. ω0 = 0.054 Hz at Day 15 and 0.08 Hz at Day 44. G′ (open symbols); G″ (filled symbols).