Published in final edited form as: Biomaterials. 2009 Aug 21;30(32):6426–6434. doi: 10.1016/j.biomaterials.2009.08.012

Figure 3.

Figure 3

SEM micrographs of macroporous and partially nanofibrous PLLA/PLGA scaffolds, phase separated in THF at -20°C (PLGA:PLLA=25:75). The total polymer concentration was 10w/v%. Original magnification: 100x for A; 5,000x for B.