Skip to main content
. Author manuscript; available in PMC: 2010 Nov 1.
Published in final edited form as: Biomaterials. 2009 Aug 21;30(32):6426–6434. doi: 10.1016/j.biomaterials.2009.08.012

Figure 7.

Figure 7

Serum protein adsorption on macroporous scaffolds with different pore wall surface architectures. (A) PLLA scaffolds phase separated in different solvents: Nano - nanofibrous, phase separated in THF at -20°C; Micro-(-196 C) - microporous, phase separated in dioxane in liquid nitrogen; Micro-(-20°C) - microporous, phase separated in dioxane at -20°C; Solid - solid-walled, generated by solvent evaporation from the polymer solution in dichloromethane; (B) PLLA/PDLLA partially nanofibrous scaffolds with different PLLA wt% in polymer blends, phase-separated in THF at -20°C.