Figure 5.

Figure 5

Scaffold fabrication. The scaffolds were fabricated using a modified salt fusion-salt leaching method. The mold is held by magnets only for easy assembly and disassembly and to present a flush top surface to produce scaffolds of uniform thickness. The lyophilized scaffolds were bored using 120 W CO2 laser to generate a regular array of microchannels. Not drawn to scale.