TABLE 1.

Composition of the PE-GNR assemblies employed in the current investigation.

First Layer Polyelectrolyte Polyelectrolyte Concentration (mg/mL) Second Layer Polyelectrolyte Polyelectrolyte Concentration (mg/mL)
PSS 2 EGDE-3,3′ 0 0.2 0.4 1 2 3
PSS 2 25kDa pEI 0.2 0.4 1 2 3 4