Skip to main content
. Author manuscript; available in PMC: 2009 Nov 11.
Published in final edited form as: J Biomech. 2008 Dec 6;42(2):158–163. doi: 10.1016/j.jbiomech.2008.10.020

Figure 1.

Figure 1

Loading protocol applied to the infraspinatus tendon. After preconditioning, the infraspinatus tendon was cyclically loaded to increasing load levels in 60N increments until failure at a rate of 0.04 mm/sec.