Fig. 4.

Fig. 4

TEM micrographs on synthesized magnetite, (a) bar = 10 nm, shows that bulk of the nanoparticles synthesized are of uniform size with few aggregates (b) bar = 5 nm scale, a magnified image of shows that an aggregate is a collection of nanoparticles with different lattice structures.