FIG. 8.

FIG. 8.

NO produced by CB-EPCs and HAECs. NO was measured, by total amount of nitrites and nitrates, in the supernatant of CB-EPCs and HAECs on FN-coated Teflon-AF or SMCs either exposed to 15 dyn/cm2 of shear stress for 24 h or under static conditions, *p < 0.001, compared to static conditions (n = 4).