Figure 5.

Figure 5

(A) T1w images of CION with and without surfactant cross-linking at different loadings between 0.5% and 3.0%, (w/v) of magnetite in 96-well plastic dish in DI water in spaces surrounding the wells. (B) T1w-TSE image illustrates apparent, concentration dependent, contrast with 0.5% CION at low nM nanoparticle concentrations.