. 2009 Dec 8;10(12):5257–5284. doi: 10.3390/ijms10125257

Figure 5.

Figure 5.

Free surface morphology and cross-section fracture of PPy film synthesized in the electrolyte of IPA + 5% BFEE + 5% PEG1000 at 15 °C.

(a) Surface morphology

(b) Cross-section fracture