Skip to main content
. 2006 Jun;97(6):985–991. doi: 10.1093/aob/mcl068

Table 1.

A comparison of E. curvula leaves (first 100 mm from base) either fully hydrated (FH) or dried to below the turgor loss point of the leaves (<TLP)

σm (MPa) W (J cm–3) E (MPa) ɛf (%)
FH 23·73 ± 9·4 0·399 ± 0·21 1051·47 ± 335·7 2·78 ± 0·5
<TLP 42·68 ± 17·2 0·739 ± 0·35 1787·09 ± 683 2·91 ± 0·4

Tensile strength (σm), toughness (W), elastic modulus (E) and failure strain (ɛf), n = 20 laminas per treatment. Values = means ± s.d. All comparisons are significantly different (P < 0·001), except for failure strain.