Skip to main content
. 2009 Dec 4;76(3):942–944. doi: 10.1128/AEM.02765-09

TABLE 1.

Resistance to and uptake of tellurite in the mutant strain carrying the plasmids used in this work

Strain Tellurite resistance (OD660)a Tellurite uptake (% of wild type)b
B100-5 NG 100
RTE36-5 1.126 ± 0.047 22.1 ± 3.3
RTE36-32 (actP) NG 113.7 ± 11.7
RTE36-40 (acs + actP) NG 142.84 ± 23.6
RTE36-42 (acs) 1.083 ± 0.018 19.08 ± 1.34
RTE36-320 (actP) NG 126.0 ± 11.6
a

Resistance was measured as optical density at 660 nm (OD660) reached by liquid cultures after 48 h, in the presence of 50 μM TeO32−. NG, no growth.

b

Tellurite uptake was measured in the presence of 100 μM TeO32−. The wild-type uptake rate, corresponding to 100%, is 4.274 ± 0.203 nmol/mg protein/min.