Skip to main content
. 2009 Feb 27;15(3):463–474. doi: 10.1089/ten.tec.2008.0431

FIG. 5.

FIG. 5.

FIG. 5.

Scanning electron microscopy (SEM) image of the cross section of mpPLLAm (57.1/42.9 wt%). (A) An angled cross section of the air-cured side of the membrane. (B) An angled cross section of the glass-cured side of the membrane. (C) The crumpled edge effects introduced by the compressional pressure applied during sectioning of the specimen.