Skip to main content
. Author manuscript; available in PMC: 2010 Mar 8.
Published in final edited form as: Adv Funct Mater. 2010;20(1):131–137. doi: 10.1002/adfm.200901311

Figure 3.

Figure 3

The effect of pre-filled precursor concentration on hydrogel gradient formation (backward flow time: 30 min). A-C) fluorescent images of hydrogel with 0%, 2% and 5% PEG-DA respectively as pre-filled solution after demolding; D-F) phase image of gradient with 0%, 2% and 5% PEG-DA solution as pre-filled solution respectively; G-H) normalized fluorescence distribution before and after demolding. Scale of figure 3a-c is 2mm and that of figure 3d-f is 300μm