Skip to main content
. Author manuscript; available in PMC: 2011 Mar 1.
Published in final edited form as: Anal Chem. 2010 Mar 1;82(5):1634–1642. doi: 10.1021/ac901955d

Figure 8.

Figure 8

Atomic force microscopy topography images (0.5 × 0.5 μm2) of 60 nm thick gold films deposited on the silicon cantilevers at (a) 0.02 nm/s, (b) 0.2 nm/s, and (c) 0.3 nm/s. Reprinted with permission from the American Institute of Physics.