Skip to main content
. 2010 Feb 1;107(8):3293–3298. doi: 10.1073/pnas.0906501107

Fig. 1.

Fig. 1.

Design of PAs for articular cartilage regeneration. Chemical structure of (A) TGF-binding PA and (B) nonbioactive filler PA. (C) Illustration of coassembly of the TGF-binding PA and the filler PA showing binding epitopes exposed on the surface of the nanofiber. (D) ELISA results showing TGFβ-1 release up to 72 hours from filler PA and 10 mol% TGF-binding PA (TGFBPA). 100 ng/mL of TGFβ-1 were loaded in all gels. Error bars equal standard deviation, n = 4.