Published in final edited form as: Electroanalysis. 2006 Jul 1;18(13-14):1254–1265. doi: 10.1002/elan.200603539

Fig. 6.

Fig. 6

Influence of the membrane thickness (left, 33 wt % PVC) and the PVC contetnt (right, membrane thickenss 150 μm) on the response of Ca2+-selective ISEs with 10−3 M CaCl2, 5 × 10−2 M Na2EDTA, pH 5. as inner solution (cf. [38]).