Table I.
Acronym |
Tg (°C) a |
Tc1 (°C) b |
Tc2 (°C) b |
Tm1 (°C) c |
Tm2 (°C) c |
Td (°C) d |
σ (mS cm−1)e |
Electrochemical window (V vs Li+/Li) |
---|---|---|---|---|---|---|---|---|
PP24TFSI | −74 | −40 | −16 | 2 | 11 | 381 | 0.77 | 1.8–4.5 |
LiTFSI–PP24TFSI | −84 | - | - | - | 5 | 374 | 0.56 | 1.5–4.5 |
Glass-transition temperature determined by DSC on heating.
Crystallization temperature determined by DSC on heating.
Melting point determined by DSC on heating.
Decomposition temperature determined by TGA.
Conductivity at 25°C.