. 2010 Mar 31;2010:456240. doi: 10.1155/2010/456240

Table 1.

Amount of extracellular matrix constituents inside hydroxyapatite.

Matrix protein total coating after 22 days of culture in fg/(cell × disk)
Static culture Ultrasonic culture Ultrasonic /Static
Decorin 5.58 ± 0.22 15.25 ± 0.42 2.73-fold
Osteocalcin 1.79 ± 0.33 5.76 ± 0.39 3.22-fold
Osteopontin 1.75 ± 0.73 3.04 ± 0.47 1.74-fold
Type-I collagen 3.72 ± 0.49 16.85 ± 0.95 4.53-fold
Type-III collagen 4.59 ± 0.13 11.04 ± 0.71 2.40-fold

Table note: P < .05 in all “Static” versus “Ultrasonic” comparisons.