. 2010 Feb 20;11(1):253–266. doi: 10.1208/s12249-010-9378-z

Fig. 7.

Fig. 7

Photos of polyvinyl acetate–polyvinyl pyrroloidone matrices exposed to (D) dry and (H) humid (75% RH) thermal stress (60°C) conditions for periods of 1 h and 1 month after dissolution testing for 12 h