Skip to main content
. Author manuscript; available in PMC: 2011 May 7.
Published in final edited form as: J Biomech. 2010 Feb 12;43(7):1408–1416. doi: 10.1016/j.jbiomech.2009.09.057

Figure 5.

Figure 5

Burst pressures for the various AAA models examined. On average, the AAA models created using the weaker silicone rubber (Sylgard 170) ruptured at lower pressures than those made using the stronger silicone (Sylgard 160).