Skip to main content
. Author manuscript; available in PMC: 2010 Apr 21.
Published in final edited form as: Biomaterials. 2005 Aug 10;27(5):735–744. doi: 10.1016/j.biomaterials.2005.06.020

Table 1.

Tensile Properties of SMC microintegrated PEUU

Sample Initial modulus (MPa) 100% modulus (MPa) Tensile strength (MPa) Breaking strain (%)
e-PEUU (random) 2.5 ± 1.2 2.8 ± 1.1 8.5 ± 1.8 280 ± 40
μSMC-e-PEUU (preferred) 1.7 ± 0.2 1.4 ± 0.2 6.5 ± 1.6 850 ± 200
μSMC-e-PEUU (cross-preferred) 0.3 ± 0.1 2.0 ± 0.5 1700 ± 100

e = electrospun scaffold; μSMC = SMC microintegrated.