Skip to main content
. Author manuscript; available in PMC: 2010 Apr 21.
Published in final edited form as: J Electrochem Soc. 2009;156(8):B943–B954. doi: 10.1149/1.3143122

Table II. OCP, maximum current density, and maximum power output of the water-equilibrated C12mimBETI (120°C) and C12imBETI (140°C) RTILs with the cathode and anode in an Ar atmosphere. (Data from Table I is shown for direct comparison.).

OCP
(mV)
Maximum current
density
(μA cm−2)
Maximum power
output
(μW cm−2)
C12mim
BETI
C12im
BETI
C12mim
BETI
C12im
BETI
C12mim
BETI
C12im
BETI
O2 cathode
H2 anodea
344 ± 62 360 ± 29 6.84 ± 3.13 37.81 ± 12.64 0.42 ± 0.18 3.40 ± 0.98
Ar cathode
Ar anode
6 ± 1 1 ± 1 0 0 0 0
a

From Table I.