Skip to main content
. 2010 Apr 26;11(4):1870–1877. doi: 10.3390/ijms11041870

Table 1.

Characterization of the polymers.

Polymers Mn a) Mw b) PDI b) Tg (°C)
PC-S c) 2490 3680 1.48 27.7
PUR-PC 5460 8270 1.52 53.3
PC-S’ 3153 3996 1.267 38.6
PUR-PC’ 8234 14532 1.765 55.2
PUR 24380 57680 2.37 44.7
a)

Calculated by SEC results;

b)

The polydispersity index, PDI = Mw/Mn;

c)

The soft segment of PUR-PC, LLA/PC molar ratio in feed was 33/1.