Pre-exposure to high-shear stress, 40 s duration. Platelets were pre-exposed to shear stresses of 1 (control), and 70 dyne/cm2, as shown in the top bar, followed by exposure to 1 dyne/cm2 for 59 min. The means of four experiments are shown ±SEM.