Skip to main content
. Author manuscript; available in PMC: 2011 Apr 19.
Published in final edited form as: Inorg Chem. 2010 Apr 19;49(8):3573–3583. doi: 10.1021/ic901814f

Figure 6.

Figure 6

Fiber-optic UV–vis spectra of an O2 calcined (450°C) Cu-ZSM-5 (Si/Al=12, Cu/Al=0.54) during reaction with CH4 at a heating rate of 10 °C/min from RT up to 225 °C. The time interval between two spectra is 1.5 min or a temperature difference of 15 °C. Reprinted from 82 with permission from Elsevier.