Published in final edited form as: J Biomed Mater Res B Appl Biomater. 2010 Jul;94(1):250–255. doi: 10.1002/jbm.b.31649

Table 3.

Micromechanical properties of the resin-dentin bonded treated interfaces using microtensile bond strength [mean (standard deviation)].

Microtensile bond strength (MPa)
24 hours 12 months
Control EDC/NHS Control EDC/NHS
One Step
Plus
41.61 (13.24)a 46.85 (13.24)a 20.84 (11.97) b 43.15 (14.16) a
Adper Single
Bond
51.72 (17.71)A 52.37 (11.39)A 26.63 (13.42) C 39.44 (17.24) B

Lower and upper case letters indicate statistically significant differences (p < 0.05) among One Step Plus and Adper Single Bond groups, respectively.

EDC: Carbodiimide; NHS: N-Hydroxysuccinimide.