FIGURE 6.

FIGURE 6

Fibronectin adsorption on poly-VAA film with 3.6, 6.2 or 9% —COOH surface densities (a), or on poly-VAA film (9% —COOH) with the thickness of 25–200 nm. N = 4, *: p < 0.05 compared to untreated TCPS.